We are using Toyo Inks to produce specials colours to tight Lab compliance. My printers are achieving good DE0.5 values when printed but are finding a significant dry back that takes them way out of tolerence 3-4 days later. Any ideas please?
 
is the sheet Aqueous or UV coated?
When we did our press we ran the samples about .05 points heavy and checked the ⌂E with dryback a few days later to determine our wet densities.
 
  • I've also found that tough tex series of toyo ink drys back much more than other series of toyo product. Is it tough tex that your using?
     
    Forum posts represent the experience, opinion, and view of individual users. The Color Printing Forum does not necessarily endorse nor share the view of each individual post. When making any potentially dangerous or financial decision, always employ and consult appropriate professionals. Your circumstances or experience may be different.