    Any ideas on what can be the cause of this Halo effect in acrylic gold?
    Job color sequence is KCMY+Aqueous coating+acrylic gold.
    This is not happening with the coating from different manufacturer. Can this be a Viscosity issue? .... IMG_20151013_153111.jpg
     
  2. turbotom1052

    turbotom1052 Senior Member

    Joined:
    Oct 2008
    Messages:
    1,044
    Location:
    Vermont
    Gold should go down first with a healthy dose of water repellent varnish or binding varnish to build up the tack. Also you may want to minimize trap in your prepress software.
     
  3. aqazi81

    aqazi81 Senior Member

    Joined:
    Oct 2009
    Messages:
    827
    Location:
    KARACHI PAKISTAN
    Its a water based gold in last coating unit and aqueous coating in 1st coating unit....machine is a Heidelberg CD 6+LYYL
     
  4. turbotom1052

    turbotom1052 Senior Member

    Joined:
    Oct 2008
    Messages:
    1,044
    Location:
    Vermont
    AHHHH my bad Aquazi, Just re read and you did mention the sequence. Cant help you as I've never worked with multiple coating units, but as you mentioned in original post it does sound like some sort of viscosity issue.
     
  5. spikeboy

    spikeboy Senior Member

    Joined:
    Sep 2014
    Messages:
    62
    Location:
    new york
    coating should go down last or am i reading this wrong
     
  6. aqazi81

    aqazi81 Senior Member

    Joined:
    Oct 2009
    Messages:
    827
    Location:
    KARACHI PAKISTAN
    Yeah I thought it too but this is how those guys are printing this job for a year or so....
     
  7. aqazi81

    aqazi81 Senior Member

    Joined:
    Oct 2009
    Messages:
    827
    Location:
    KARACHI PAKISTAN
    @turbotom..... I never worked on a dual coater too that's why I posted here to get some expert opinion.... the only thing that I can figure out is the viscosity.
     

  8. charlie wishon

    charlie wishon Member

    Joined:
    Oct 2011
    Messages:
    15
    Location:
    rogers ar U.S.A
    could be a gassing issue between coatings. what type of coating are you laying down 1st ? work, and turn. high gloss/high rub, satin ?
     